2017
DOI: 10.14382/epitoanyag-jsbcm.2017.3
|View full text |Cite
|
Sign up to set email alerts
|

The effect of the alkaline solution content on the mechanical properties of MK-based PVA fiber-reinforced geopolymers

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1

Citation Types

0
3
0

Year Published

2018
2018
2023
2023

Publication Types

Select...
4

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(3 citation statements)
references
References 19 publications
0
3
0
Order By: Relevance
“…During curing in solution, they undergo distinct processes of formation via: (a) dissolution, (b) polycondensation; and (c) precipitation 3,4 . Several designs have been evaluated in the literature, 2,3,5,6 and their main formulation is based on M 2 O•Al 2 O 3 •xSiO 2 •yH 2 O 1,5 ; where M represents the alkali (Na or K); and x and y are determined according to the molar ratios desired. Their applications have been growing in recent years, encompassing different purposes and markets, such as: (a) fire‐resistant structures; 3,7 (b) nuclear waste encapsulation 4,7 ; (c) alternatives to cement‐based materials 8,9 …”
Section: Introductionmentioning
confidence: 99%
“…During curing in solution, they undergo distinct processes of formation via: (a) dissolution, (b) polycondensation; and (c) precipitation 3,4 . Several designs have been evaluated in the literature, 2,3,5,6 and their main formulation is based on M 2 O•Al 2 O 3 •xSiO 2 •yH 2 O 1,5 ; where M represents the alkali (Na or K); and x and y are determined according to the molar ratios desired. Their applications have been growing in recent years, encompassing different purposes and markets, such as: (a) fire‐resistant structures; 3,7 (b) nuclear waste encapsulation 4,7 ; (c) alternatives to cement‐based materials 8,9 …”
Section: Introductionmentioning
confidence: 99%
“…The specimens containing fibres exhibited higher fracture toughness and ductility. Xu et al [24] Borges et al [54] blended MK with SF to reach molar ratios of 3, 3.4 and 3.8. The composites were mixed with very fine sand and activated with NaOH and sodium silicate solutions.…”
Section: Blended Geopolymersmentioning
confidence: 99%
“…Borges et al [54] blended MK with SF to reach molar ratios of 3, 3.4 and 3.8. The composites were mixed with very fine sand and activated with NaOH and sodium silicate solutions.…”
Section: Pva Fibresmentioning
confidence: 99%