2022
DOI: 10.1134/s0021364022600720
|View full text |Cite
|
Sign up to set email alerts
|

Temperature Dependence of the Fano Resonance in Nanodiamonds Synthesized at High Static Pressures

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1

Citation Types

0
3
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
5

Relationship

0
5

Authors

Journals

citations
Cited by 5 publications
(3 citation statements)
references
References 24 publications
0
3
0
Order By: Relevance
“…Only for MND-H, a dip in the absorbance is visible at 1330 cm –1 . This particularity is the focus of recent studies, attributing this phenomenon to a surface conductivity of MND-H in water. , Note that for both MND-H and MND-Ox samples, bands located at ca . 3300 and 1620 cm –1 associated, respectively, with the O–H stretching and bending modes may be partially or totally related to the presence of water molecules since infrared measurements were performed under air at ambient temperature.…”
Section: Resultsmentioning
confidence: 92%
“…Only for MND-H, a dip in the absorbance is visible at 1330 cm –1 . This particularity is the focus of recent studies, attributing this phenomenon to a surface conductivity of MND-H in water. , Note that for both MND-H and MND-Ox samples, bands located at ca . 3300 and 1620 cm –1 associated, respectively, with the O–H stretching and bending modes may be partially or totally related to the presence of water molecules since infrared measurements were performed under air at ambient temperature.…”
Section: Resultsmentioning
confidence: 92%
“…Later, high temperature and pressure techniques were developed for synthesizing NDs . The static-pressure catalyst method can be used for synthesizing NDs at a constant ultrahigh pressure and high temperature with a catalyst . If a catalyst is not used, higher pressures and temperatures are required.…”
Section: Methods For Synthesizing 0d Cnmsmentioning
confidence: 99%
“…176 The static-pressure catalyst method can be used for synthesizing NDs at a constant ultrahigh pressure and high temperature with a catalyst. 177 If a catalyst is not used, higher pressures and temperatures are required. Although high-energy ball-milling somewhat compensates for the safety of the high temperature and pressure method, the equipment parts and ball-milling media are easily damaged, and the impurity content of the dispersed particles is too high owing to the high hardness and wear resistance of the diamond material.…”
Section: Preparation and Design Principlementioning
confidence: 99%