Temperature dependence of energy transfer in tunable white light-emitting phosphor BaY2Si3O10:Bi3+,Eu3+ for near UV LEDs

Abstract: The white light emission of BaY2Si3O10:0.01 Bi3+, mEu3+ phosphor can be realized and utilizing the energy transfer under near UV light pumped. The energy transfer efficiency between Bi(i) and Bi(ii) change with the temperature increasing due to phonon-assisted process. It is rare in the experiment on directly proof with the phonon-assisted energy transfer.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
41
1

Year Published

2017
2017
2020
2020

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 93 publications
(45 citation statements)
references
References 40 publications
1
41
1
Order By: Relevance
“…Broad excitation band from 200 to 450 nm was observed monitored at 616 nm. The strongest peak at about 270 nm is ascribed to Eu 3+ −O 2− charge transfer transition (CTB) from negative oxygen 2p orbit to the empty 4f orbit of Eu 3+ , which is easy to influence by host environment [27]. Other narrow absorption peaks in the regionof 300 to 450 nm at 363, 382, 394, and 467 nm are attributed to 7 F 0 → 5 D 4 , 7 F 0 → 5 G 4 , 7 F 0 → 5 L 6 , and 7 F 0 → 5 D 2 transitions, respectively.…”
Section: Resultsmentioning
confidence: 99%
“…Broad excitation band from 200 to 450 nm was observed monitored at 616 nm. The strongest peak at about 270 nm is ascribed to Eu 3+ −O 2− charge transfer transition (CTB) from negative oxygen 2p orbit to the empty 4f orbit of Eu 3+ , which is easy to influence by host environment [27]. Other narrow absorption peaks in the regionof 300 to 450 nm at 363, 382, 394, and 467 nm are attributed to 7 F 0 → 5 D 4 , 7 F 0 → 5 G 4 , 7 F 0 → 5 L 6 , and 7 F 0 → 5 D 2 transitions, respectively.…”
Section: Resultsmentioning
confidence: 99%
“…Meanwhile, the rotation speed of the mill is 200 rpm and ball‐milling time is 10 hours. After mixing and drying, a small amount of powders were pressed into plates of 15 mm diameter and 1.5 mm thickness; then, the plates were embedded into powders of each composition for presintering at 780‐1000°C for 3 hours . During the presintering process, the major reaction was as follows:Na2CO3+Bi2O3+4TiO24false(Bi0.5Na0.5false)TiO3+CO2false↑…”
Section: Methodsmentioning
confidence: 99%
“…Typically, Bi‐doped materials can be developed as phosphors to radiate from UV to IR region . Therefore, in this paper, we have studied Eu 3+ ‐doped BNT ceramic in order to improve its electrical properties and achieve excellent luminescence properties …”
Section: Introductionmentioning
confidence: 99%
“…Meanwhile, with the development of LED chip technology, the emission bands of LED chips shifted from blue light to near-UV range which can offer higher energy to pump the phosphor 9 . For the above reasons, more and more attentions have been paid on phosphors with high absorption in the near-UV spectral region 1012 .…”
Section: Introductionmentioning
confidence: 99%