Technological study of iron ore processing from Chandmani-Uul deposit by dry and wet magnetic separation

Abstract: The iron ore sample is processed in laboratory conditions with methods of both dry and wet magnetic separation. The particle size of the processed sample was 1 mm electric power of dry magnetic separation 0.2A-0.6A, and the rotation number of the separation drum was chosen to be 32 per/min. The most suitable procedures to get standardized concentrate are optimized through considering the following facts that the duration of wet magnetic separation is 20, 30, 40, 50 minutes, classification yield is 43.50 %, 55.… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2021
2021
2024
2024

Publication Types

Select...
1
1

Relationship

0
2

Authors

Journals

citations
Cited by 2 publications
(1 citation statement)
references
References 0 publications
0
1
0
Order By: Relevance
“…The total resources are calculated at 5.5 billion tons. About 300 deposits, occurrences, and mineralization points with an average iron content of 20-55% have been identified [1]. Mongolia exports iron concentrate with 62-65% iron content by primary processing of iron ore.…”
Section: Introductionmentioning
confidence: 99%
“…The total resources are calculated at 5.5 billion tons. About 300 deposits, occurrences, and mineralization points with an average iron content of 20-55% have been identified [1]. Mongolia exports iron concentrate with 62-65% iron content by primary processing of iron ore.…”
Section: Introductionmentioning
confidence: 99%