Synthesis of octahydro-2H-chromen-4-ol from vanillin and isopulegol over acid modified montmorillonite clays: Effect of acidity on the Prins cyclization

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

4
24
0

Year Published

2016
2016
2024
2024

Publication Types

Select...
6
1

Relationship

1
6

Authors

Journals

citations
Cited by 38 publications
(29 citation statements)
references
References 19 publications
4
24
0
Order By: Relevance
“…Presence of Na + in the montmorillonites from the Taganskoye deposit was also confirmed in previous studies [26,42,43]. (Figure 1).…”
Section: Transformation Of the Montmorillonite Structure Under Acid Tsupporting
confidence: 89%
See 2 more Smart Citations
“…Presence of Na + in the montmorillonites from the Taganskoye deposit was also confirmed in previous studies [26,42,43]. (Figure 1).…”
Section: Transformation Of the Montmorillonite Structure Under Acid Tsupporting
confidence: 89%
“…Early, we demonstrated that the chemical composition and structural characteristics of Mt depended on the HNO 3 and HCl concentration [26,32]. Changes of chemical composition and interlayer space were negligible after modification of montmorillonite under the concentrations up to 0.5 M. These changes were noticeable only after treatment with 3.0 M acid.…”
Section: Transformation Of the Montmorillonite Structure Under Acid Tmentioning
confidence: 87%
See 1 more Smart Citation
“…Also, this fact was confirmed by the EDX data (Tab. 2), and described in previous studies of the bentonites from Taganskoye deposit [12,13]. Treatment of Mt-M sample with hydrochloric acid solution with various concentrations leads to partial protonation of interlayer, which is observed by a decrease of d00l values and changes of basal reflections series from d001 = 15.3Å, d003 = 5.0Å, d005 = 3.0Å to d001 = 13.7Å.…”
Section: Introductionmentioning
confidence: 75%
“…2a) after the treatment of Mt-T2 sample with HNO3 acid for 108 hours. Previous studies of Mt-М and Мt-Т1 samples treated with HCl acid [13] showed the reduction of bands intensity at 841-845 cm -1 (Al-Mg-OH), 882 cm -1 (Al-Fe-OH) and 914-926 cm -1 (Al-Al -OH), which indicates the leaching of Al 3+ , Mg 2+ and Fe 3+ cations from the octahedral sites [14,17,18,19,20]. Reduction of the band intensities at 925 and 876 cm-1 is shown at Fig.…”
Section: Introductionmentioning
confidence: 99%