2011
DOI: 10.1016/j.physb.2011.02.044
|View full text |Cite
|
Sign up to set email alerts
|

Synthesis, characterization and photoelectrochemical properties of n-CdS thin films

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

5
18
0

Year Published

2013
2013
2022
2022

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 49 publications
(23 citation statements)
references
References 32 publications
5
18
0
Order By: Relevance
“…ρ = ρo exp (-ΔE /KT) ... (7) The activation energy was found to be in the range of 0.215 to 0.336 eV. Similar finding were reported by different researchers for CdS thin films [13,14] Thermoemf Measurement of Cd x Zn 1-x S Films.…”
Section: Electrical Characterization Of CD X Zn 1-x S Thin Filmssupporting
confidence: 70%
“…ρ = ρo exp (-ΔE /KT) ... (7) The activation energy was found to be in the range of 0.215 to 0.336 eV. Similar finding were reported by different researchers for CdS thin films [13,14] Thermoemf Measurement of Cd x Zn 1-x S Films.…”
Section: Electrical Characterization Of CD X Zn 1-x S Thin Filmssupporting
confidence: 70%
“…Therefore, more extensive studies on the nanoforms of CdS semiconductor and their various properties have been carried out. A variety of chemical routes to synthesize CdS nanoforms have been employed [6,9,[14][15][16][17][18][19][20][21][22]. However, the co-precipitation technique is an important bottomup approach for the synthesis of nanoparticles.…”
mentioning
confidence: 99%
“…Throughout the deposition process S/Cd decreased gradually. The grain size of the film was calculated from the line broadening in the XRD pattern by using Scherer's formula [5,6] and is shown Table 1. The 5 min KMnO 4 substrate activated CdS thin film is amorphous in nature as shown in Figure 1.…”
Section: Preparation Of Thin Filmsmentioning
confidence: 99%
“…Figure 2(a) shows the optical absorption for substrate activation time, and the maximum peak was observed at 15 min. A Tauc plot ( ℎ]) 2 as function of photon energy (ℎ]) for CdS thin films with various substrate activation time is shown in Figure 3 [6,7], and the optical energy gaps are shown in Table 1. There is a change in CdS band gap due to a change in different KMnO 4 activation time conditions [8].…”
Section: Optical Studies (Uv Spectral Analysis)mentioning
confidence: 99%