Synthesis and properties of soybean oil-based biodegradable polyurethane films

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
24
0
2

Year Published

2018
2018
2023
2023

Publication Types

Select...
9

Relationship

3
6

Authors

Journals

citations
Cited by 56 publications
(30 citation statements)
references
References 57 publications
0
24
0
2
Order By: Relevance
“…The main reason for this behavior could probably be explained by its highest hydrophilicity and molar ratio of PLA, providing a larger amount of ester bonds than others. These bonds were subjected to scission by lipase and more hydrophilic nature that increase the interactions of water with the graft copolymers PLA%=100[]()1+2+3+5+6+7+8+9+1018f3+1+2+3+5+6+7+8+9+1018×100 …”
Section: Resultsmentioning
confidence: 99%
“…The main reason for this behavior could probably be explained by its highest hydrophilicity and molar ratio of PLA, providing a larger amount of ester bonds than others. These bonds were subjected to scission by lipase and more hydrophilic nature that increase the interactions of water with the graft copolymers PLA%=100[]()1+2+3+5+6+7+8+9+1018f3+1+2+3+5+6+7+8+9+1018×100 …”
Section: Resultsmentioning
confidence: 99%
“…This ingredients such as chitosan [580], silver nanoparticles [581] and iodine [582]. [58,389,476,581,586,[622][623][624][625][626][627][628][629], polyethylene butylene adipate (PEBA) [587,608], lignin [623], gelatin [602], chitin/chitosan [630,631], collagen [632], alginate [633] and heparin [634]. It is noteworthy that PUs with adequate biodegradability may still present excellent…”
Section: Biodegradation Of Polyurethane Elastomersmentioning
confidence: 99%
“…After the hydrogel sample was removed from the degradation solution, it was cleaned with deionized water and dried at 50°C under vacuum for 24 hours. The weight loss of PAMU‐ and CS‐based hydrogel sample was calculated using Equation : Weight loss0.25em()%=()WbeforeWafterWbefore×100, where W after and W before are the weights of the hydrogels after and before in vitro biodegradation.…”
Section: Methodsmentioning
confidence: 84%