Synthesis and photocatalytic activity of mesoporous g-C 3 N 4 /MoS 2 hybrid catalysts

Abstract: The key to solving environmental and energy issues through photocatalytic technology requires highly efficient, stable and eco-friendly photocatalysts. Graphitic carbon nitride (g-C3N4) is one of the most promising candidates except for its limited photoactivity. In this work, a facile and scalable one-step method is developed to fabricate an efficient heterostructural g-C3N4 photocatalyst in situ coupled with MoS2. The strong coupling effect between the MoS2 nanosheets and g-C3N4 scaffold, numerous mesopores … Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
12
0

Year Published

2019
2019
2022
2022

Publication Types

Select...
8
1

Relationship

0
9

Authors

Journals

citations
Cited by 37 publications
(13 citation statements)
references
References 64 publications
1
12
0
Order By: Relevance
“…The XRD pattern of the Mg-Al LDH and g-C 3 N 4 , sample is in good agreement with the JCPDS card no: 35-0965 [37] and 87-1526 [38], respectively. The diffraction peaks indexed to (003), (006), (012), (015), (018), and (110) are the plane reflections of a typical hydrotalcite-like phase screening, sharp and symmetric basal (00 l) reflection of LDH.…”
Section: Structural Investigationsupporting
confidence: 81%
“…The XRD pattern of the Mg-Al LDH and g-C 3 N 4 , sample is in good agreement with the JCPDS card no: 35-0965 [37] and 87-1526 [38], respectively. The diffraction peaks indexed to (003), (006), (012), (015), (018), and (110) are the plane reflections of a typical hydrotalcite-like phase screening, sharp and symmetric basal (00 l) reflection of LDH.…”
Section: Structural Investigationsupporting
confidence: 81%
“…Graphitic carbon nitride nanosheets (C 3 N 4 ) were synthesized with urea (20 g) in a vacuum tube furnace. The ramping rate was 5 °C/min, and the temperature was kept at 550 °C under nitrogen flow for 4 h [ 47 ]. The synthesized C 3 N 4 was cooled down to ambient temperature in the vacuum tube furnace and then washed with deionized water three times.…”
Section: Methodsmentioning
confidence: 99%
“…12,[25][26][27] Selected examples for CN composites comprise MoS 2 /C 3 N 4 , Bi 2 WO 6 /C 3 N 4 , Ag/C 3 N 4 , Fe 3 O 4 /C 3 N 4 and a-Fe 2 O 3 /C 3 N 4 . 12,15,22,28,29 However, these investigations are based on dispersions of particles, and their use requires an additional costly process step for particle separation in any technologically relevant approach. Although, dispersions show generally signicant higher activities than immobilized particles, it is essential to establish photocatalytic processes using immobilized photocatalysts.…”
Section: Introductionmentioning
confidence: 99%