Abstract:Lead Sulphide (PbS) thin film was deposit by chemical bath deposition (CBD) process on the glass substrate at room temperature for various time intervals. The precursors used for this deposition are lead acetate since as a supply of lead ions (Pb2+) and thiourea the same as the supply of sulfide ions (S2-) with 0.1M concentration. The pH of the mixed precursors solution was maintained at 9.5-10 by addition of drop by drop ammonia very slowly. The cause of deposition time for different hours studied. The influe… Show more
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.