“…These values were comparable to those previously reported of CdSe films at around 202 AE 3 cm À1 (LO W-CdSe). 55 Second-and third-phonon modes (2LO and 3LO) were clearly observed at 408 and 614 cm À1 for 6F and at 413 and 619 cm À1 for 6Fb.…”
Section: Raman Spectroscopy (Rs)mentioning
confidence: 94%
“…1,45 The hexagonal phase is commonly observed for ternary materials, although a mixture of both cubic and hexagonal phases are reported. 55 Annealed 3Fa exhibited growth along the (002) plane, while 5Fa seemed to lose preferential plane orientations.…”
Section: Structural Analysis Of Thin Filmsmentioning
confidence: 98%
“…On the other hand, the average composition can be easily estimated based on the observed LO phonon frequencies ( ω LOCdS / ω LOCdSe ) and comparison with those of bulk crystals. 55 The av. composition can also be estimated by plotting the difference between the observed CdS-like and CdSe-like LO phonon frequencies ( ω LOCdS − ω LOCdSe ).…”
Homoleptic Zinc(II) and cadmium(II) complexes containing hybrid N-selenophosphinoylchalcogenoureato ligands, [M(iPr₂P(Se)NC(X)NC₅H₁₀-κ²-Se,X)₂] (M = Zn, X = S (3), X = O (4) and M = Cd, X = S (5)) and...
“…These values were comparable to those previously reported of CdSe films at around 202 AE 3 cm À1 (LO W-CdSe). 55 Second-and third-phonon modes (2LO and 3LO) were clearly observed at 408 and 614 cm À1 for 6F and at 413 and 619 cm À1 for 6Fb.…”
Section: Raman Spectroscopy (Rs)mentioning
confidence: 94%
“…1,45 The hexagonal phase is commonly observed for ternary materials, although a mixture of both cubic and hexagonal phases are reported. 55 Annealed 3Fa exhibited growth along the (002) plane, while 5Fa seemed to lose preferential plane orientations.…”
Section: Structural Analysis Of Thin Filmsmentioning
confidence: 98%
“…On the other hand, the average composition can be easily estimated based on the observed LO phonon frequencies ( ω LOCdS / ω LOCdSe ) and comparison with those of bulk crystals. 55 The av. composition can also be estimated by plotting the difference between the observed CdS-like and CdSe-like LO phonon frequencies ( ω LOCdS − ω LOCdSe ).…”
Homoleptic Zinc(II) and cadmium(II) complexes containing hybrid N-selenophosphinoylchalcogenoureato ligands, [M(iPr₂P(Se)NC(X)NC₅H₁₀-κ²-Se,X)₂] (M = Zn, X = S (3), X = O (4) and M = Cd, X = S (5)) and...
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.