Sunlight driven isotropic β-Bi2O3 with high charge-carrier mobility for the efficient degradation of bisphenol A and phenol

Abstract: Nanostructure β-Bi2O3 was synthesized and used for the photocatalytic degradation of bisphenol A and phenol. After 90 minutes of sun light irradiation, the degradation efficiencies of bisphenol A and phenol...

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

1
5
0

Year Published

2022
2022
2023
2023

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 13 publications
(6 citation statements)
references
References 69 publications
1
5
0
Order By: Relevance
“…In Fig. 3(a), the Raman spectra profiles of γ-Bi 2 O 3 and Bi 2 MoO 6 were the same as those found in the literature 17,41,48 which indicated the synthesis of the pure phases of γ-Bi 2 O 3 and Bi 2 MoO 6 . These Raman peaks correspond to the symmetric and asymmetric stretching vibration of the Bi-O bonds and Mo-O bonds, respectively.…”
Section: Calculation Processsupporting
confidence: 79%
See 3 more Smart Citations
“…In Fig. 3(a), the Raman spectra profiles of γ-Bi 2 O 3 and Bi 2 MoO 6 were the same as those found in the literature 17,41,48 which indicated the synthesis of the pure phases of γ-Bi 2 O 3 and Bi 2 MoO 6 . These Raman peaks correspond to the symmetric and asymmetric stretching vibration of the Bi-O bonds and Mo-O bonds, respectively.…”
Section: Calculation Processsupporting
confidence: 79%
“…The γ-Bi 2 O 3 was prepared by the water bath heating method and a detailed description is found in papers in the literature. 17,41 The Bi 2 MoO 6 and γ-Bi 2 O 3 powders with mass proportions of 1 : 1, 1 : 2, 1 : 3, 2 : 1, and 3 : 1 were mixed and then ground in a mortar. The mixture was calcined at temperatures of 200, 300, 400, 500 °C for durations of 1, 2, 3, 4, and 5 h. The heterojunctions are showed in Table 1.…”
Section: Synthesismentioning
confidence: 99%
See 2 more Smart Citations
“…The most substantial peak at approximately 529.9 eV is typical of lattice oxygen for β-Bi 2 O 3 , whereas the other peak at 530.9 eV is associated with the adsorbed oxygen. 37,38 In comparison with pure β-Bi 2 O 3 , B2 exhibits a higher intensity of lattice oxygen and its binding energy slightly diminishes to 529.6 eV. It may imply that the two distinctive structures of Bi 2 O 3 together contribute to forming the new lattice oxygen.…”
Section: Resultsmentioning
confidence: 99%