Sugarcane hybrids with original low lignin contents and high field productivity are useful to reach high glucose yields from bagasse

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

1
26
1
23

Year Published

2016
2016
2021
2021

Publication Types

Select...
5

Relationship

0
5

Authors

Journals

citations
Cited by 32 publications
(51 citation statements)
references
References 29 publications
1
26
1
23
Order By: Relevance
“…The aim was to use alkaline sulfite pretreated samples with varied compositional characteristics to compare both groups of substrates under enzymatic hydrolysis, aiming to prepare glucose plus xylose rich syrups. Solids yield and chemical composition of alkaline sulfite pretreated samples were previously reported, showing that the yield of recovered solids was in the range of 80–97% for 5% sulfite loads and 71–89% for 7.5% sulfite loads. Decreased solid yields with increasingly sulfite loads were mainly a consequence of increased delignification efficiency .…”
Section: Resultsmentioning
confidence: 57%
See 4 more Smart Citations
“…The aim was to use alkaline sulfite pretreated samples with varied compositional characteristics to compare both groups of substrates under enzymatic hydrolysis, aiming to prepare glucose plus xylose rich syrups. Solids yield and chemical composition of alkaline sulfite pretreated samples were previously reported, showing that the yield of recovered solids was in the range of 80–97% for 5% sulfite loads and 71–89% for 7.5% sulfite loads. Decreased solid yields with increasingly sulfite loads were mainly a consequence of increased delignification efficiency .…”
Section: Resultsmentioning
confidence: 57%
“…Solids yield and chemical composition of alkaline sulfite pretreated samples were previously reported, showing that the yield of recovered solids was in the range of 80–97% for 5% sulfite loads and 71–89% for 7.5% sulfite loads. Decreased solid yields with increasingly sulfite loads were mainly a consequence of increased delignification efficiency . Figure compares components removal in alkaline and acid sulfite processes.…”