2022
DOI: 10.2139/ssrn.4207624
|View full text |Cite
|
Sign up to set email alerts
|

Study on Ablation Behavior and Mechanism of Cf/Hfcpip-Siccvi Composites: From Sio2 Nanowires Film to Hfo2 Skeleton Structure

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
2
0

Year Published

2023
2023
2023
2023

Publication Types

Select...
1

Relationship

0
1

Authors

Journals

citations
Cited by 1 publication
(2 citation statements)
references
References 0 publications
0
2
0
Order By: Relevance
“…Figure a shows the XRD patterns of two different char layers before and after ZB modification. Two broad peaks appearing at 2θ angles of 9.42 and 21.96° were attributed to SiO 2 (PDF 51-1377, 51-1379), respectively, which provides a barrier to outside gases. , Three sharp peaks observed at 2θ angles of about 35.43, 59.86, and 71.71° are the characteristic peaks of SiC (PDF #29-1129). It is speculated that SiC is produced in situ by siloxane ceramization or a carbothermal reaction, which contributes to high temperature and ablation resistance of the composites. , Besides, the characteristic peak observed at 27.75° was attributed to B 2 O 3 (PDF 06-0297), which can be presumed to be a decomposition product of ZB.…”
Section: Results and Discussionmentioning
confidence: 99%
See 1 more Smart Citation
“…Figure a shows the XRD patterns of two different char layers before and after ZB modification. Two broad peaks appearing at 2θ angles of 9.42 and 21.96° were attributed to SiO 2 (PDF 51-1377, 51-1379), respectively, which provides a barrier to outside gases. , Three sharp peaks observed at 2θ angles of about 35.43, 59.86, and 71.71° are the characteristic peaks of SiC (PDF #29-1129). It is speculated that SiC is produced in situ by siloxane ceramization or a carbothermal reaction, which contributes to high temperature and ablation resistance of the composites. , Besides, the characteristic peak observed at 27.75° was attributed to B 2 O 3 (PDF 06-0297), which can be presumed to be a decomposition product of ZB.…”
Section: Results and Discussionmentioning
confidence: 99%
“…Two broad peaks appearing at 2θ angles of 9.42 and 21.96°were attributed to SiO 2 (PDF 51-1377, 51-1379), respectively, which provides a barrier to outside gases. 60,61 Three sharp peaks observed at 2θ angles of about 35.43, 59.86, and 71.71°are the characteristic peaks of SiC (PDF #29-1129). It is speculated that SiC is produced in situ by siloxane ceramization or a carbothermal reaction, which contributes to high temperature and ablation resistance of the composites.…”