“…The pigment suspension containing 0%, 1% or 20 5% of the API was prepared through Ultra-Turrax (IKA-Werke GmbH & Co. KG, Staufen, Germany) mixing (17,500 rpm) for 10 min. After this, the suspension was poured into the polymer dispersion and mixed with an overhead stirrer (IKA-Werke GmbH & Co. KG) at 210 rpm for 15 min [66]. As a final step, the mixture was sieved.…”