Study of Mechanical and Crystalline Behavior of Polyamide 6/Hytrel/Carbon Nanotubes (CNT) based Polymer Composites

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

1
14
0

Year Published

2016
2016
2022
2022

Publication Types

Select...
5
2

Relationship

0
7

Authors

Journals

citations
Cited by 27 publications
(15 citation statements)
references
References 15 publications
1
14
0
Order By: Relevance
“…According to Table , T m increases slightly on incorporation of both ND‐COOH and ND‐EDA indicating their role in the formation of thicker and more perfect crystals . Additionally, this can be attributed to the limited segmental motion of PA6 chains in the presence of nanoparticles and also the high thermal stability of the inorganic fillers . However, only ND‐EDA increases T c and X c of PA6 which can be associated with its nucleating role .…”
Section: Resultsmentioning
confidence: 98%
See 1 more Smart Citation
“…According to Table , T m increases slightly on incorporation of both ND‐COOH and ND‐EDA indicating their role in the formation of thicker and more perfect crystals . Additionally, this can be attributed to the limited segmental motion of PA6 chains in the presence of nanoparticles and also the high thermal stability of the inorganic fillers . However, only ND‐EDA increases T c and X c of PA6 which can be associated with its nucleating role .…”
Section: Resultsmentioning
confidence: 98%
“…28,50 Additionally, this can be attributed to the limited segmental motion of PA6 chains in the presence of nanoparticles 28 and also the high thermal stability of the inorganic fillers. 51 However, only ND-EDA increases T c and X c of PA6 which can be associated with its nucleating role. 52,53 In the amorphous phase of matrix, the motions of PA6 chains contribute to heterogeneous crystalline growth in the vicinity of ND particles.…”
Section: Morphological Analysismentioning
confidence: 93%
“…Different dispersion methods for loading various polymer matrices with CNTs are designed, namely, solution blending, melt blending, in situ polymerization, latex technology, solid‐state shear pulverization, and coagulation spinning . In highly viscous melts, the most popular methods of CNTs incorporation are twin‐screw extrusion technique and roller mixing . These approaches allow increasing the mixing speed realize high shear rate and shear stress that result in broken agglomerates of filler particles and consequently higher uniformity of nanocarbon dispersion in the bulk polymer matrix.…”
Section: Introductionmentioning
confidence: 99%
“…However, the degree of crystallinity of magnesium-catalyzed cast PA6 have not yet been investigated. The degree of crystallinity for sodium-catalyzed PA6 is about 40-50% based on the literature data [32,33]. The degrees of crystallinity of magnesium-catalyzed semi-finished PA6 rods were analysed and its range between 15% and 27% was found.…”
Section: Differential Scanning Calorimetrymentioning
confidence: 99%