Structural characterisation of titania or silane-grafted TiO2-SiO2 oxide composite and influence of ionic strength or electrolyte type on their electrokinetic properties

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
6
0

Year Published

2012
2012
2023
2023

Publication Types

Select...
8

Relationship

3
5

Authors

Journals

citations
Cited by 17 publications
(6 citation statements)
references
References 25 publications
0
6
0
Order By: Relevance
“…Zeta potential is crucial for stability control of TiO 2 nanoparticles in suspensions and for the adsorption properties of TiO 2 nanoparticle surfaces. Many authors have shown that the zeta potential of particles depends on several factors, such as the chemical composition of particle surfaces, the composition of the surrounding solvent, pH value, and the presence of ions in the suspension [44][45][46][47][48][49][50]. Titania nanoparticles show a wide range of surface adsorption and optical properties which depend on their shapes and sizes and which correlate to photocatalytic activity [51][52][53][54][55].…”
Section: Introductionmentioning
confidence: 99%
“…Zeta potential is crucial for stability control of TiO 2 nanoparticles in suspensions and for the adsorption properties of TiO 2 nanoparticle surfaces. Many authors have shown that the zeta potential of particles depends on several factors, such as the chemical composition of particle surfaces, the composition of the surrounding solvent, pH value, and the presence of ions in the suspension [44][45][46][47][48][49][50]. Titania nanoparticles show a wide range of surface adsorption and optical properties which depend on their shapes and sizes and which correlate to photocatalytic activity [51][52][53][54][55].…”
Section: Introductionmentioning
confidence: 99%
“…[36][37][38] In detail, the silane was at first dispersed by ultrasound in methanol/water solution (4/1 v/v) and then hydrolyzed at room temperature for 2 h in the presence of a suitable amount of SiO 2 (30 phr, i.e. parts of hundreds of rubber).…”
Section: Preparation Of Sio 2 @Poss Hybrid Fillermentioning
confidence: 99%
“…In the second step, the obtained titania powder was grafted with AAPTS-sample TA. Modification was performed using 1 wt.% of AAPTS (calculated for 100 g of TiO 2 ) prepared in a MeOH/deionized water mixture (4/1 v/v) and applying the socalled dry technique, described in detail in [24,25]. Titania was treated with AAPTS to obtain a positively charged surface, to enhance the interaction between titania and graphene oxide.…”
Section: Preparation Of Modified Titaniamentioning