2023
DOI: 10.1016/j.mtcomm.2023.106385
|View full text |Cite
|
Sign up to set email alerts
|

Stress corrosion phenomenon of BeO at room temperature and its mechanism: Experimental and molecular dynamics study

Ming-dong Hou,
Xiang-wen Zhou,
Bing Liu
Help me understand this report