Acrylonitrile-butadiene-styrene (ABS) copolymers were synthesized in emulsions and silica-containing emulsion gels at 20, 40, and 60 °C. The room-temperature polymerization was achieved by decomposing 2,2’-azobisisobutyronitrile (AIBN) at oil-water interfaces. The...