Spark plasma sintering of (Ti0.9W0.1) C powders prepared by mechanical alloying

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
2
0

Year Published

2014
2014
2024
2024

Publication Types

Select...
3
1

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(2 citation statements)
references
References 32 publications
0
2
0
Order By: Relevance
“…In other word, the broadening of the experimental reflection peaks of the f.c.c (Ti,W)C samples is related to the small size of the diffracting grains, the lattice microstrain and the instrumental broadening. The XRD patterns analysis of Ti 0.9 W 0.1 C powders were discussed in detail in previous work [23]. Fig.…”
Section: Experimental Methodsmentioning
confidence: 99%
See 1 more Smart Citation
“…In other word, the broadening of the experimental reflection peaks of the f.c.c (Ti,W)C samples is related to the small size of the diffracting grains, the lattice microstrain and the instrumental broadening. The XRD patterns analysis of Ti 0.9 W 0.1 C powders were discussed in detail in previous work [23]. Fig.…”
Section: Experimental Methodsmentioning
confidence: 99%
“…The lattice parameter of annealed TiC is 0.43274 nm [28]. We reported in our work [23] that the composition of (Ti,W)C powder has the following formula: (Ti 0.898 W 0.101 ) C 1.09 . This formula shows clearly a carbon excess ð C Ti N0:85Þ.…”
Section: Crystallite Size and Structural Microstrainmentioning
confidence: 95%