Some aspects on workability of aluminium–iron powder metallurgy composite during cold upsetting

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
49
0

Year Published

2007
2007
2014
2014

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 70 publications
(49 citation statements)
references
References 17 publications
0
49
0
Order By: Relevance
“…The expressions for the normal stress (σz), normal strain (ɛz), hoop stress (σθ), hoop strain (ɛθ), hydrostatic stress (σm), effective stress (σeff), and effective strain (ɛeff) were taken from Selvakumar et al [7] and Narayanasamy et al [8].…”
Section: Theoretical Analysismentioning
confidence: 99%
See 1 more Smart Citation
“…The expressions for the normal stress (σz), normal strain (ɛz), hoop stress (σθ), hoop strain (ɛθ), hydrostatic stress (σm), effective stress (σeff), and effective strain (ɛeff) were taken from Selvakumar et al [7] and Narayanasamy et al [8].…”
Section: Theoretical Analysismentioning
confidence: 99%
“…Narayanasamy et al [8] have studied the strain hardening behaviour of aluminium-iron powder composite preforms. The authors performed experiments on sintered powders of three different aspect ratios, different compositions of Fe and three different particle sizes.…”
Section: Introductionmentioning
confidence: 99%
“…The compact pressure was maintained for all composition of SiC composites to maintain the 92% relative density level. The green compact surfaces were coated with an indigenously developed ceramic mixture [21] and dried under room-temperature conditions for a period of 9 h. A second coating was applied at a direction of 90°to the direction of first coating and was allowed to dry for a further period of 9 h under the same conditions as stated above.…”
Section: Compacts Preparationmentioning
confidence: 99%
“…1 Photographs of hydraulic press and parts of compacting die tool Fig. 2 The SEM photograph of as sintered Al-20% SiC at 605°C at 3 h [21,22], Fe [23], Fe-TiC [24] and Al-SiC [25] composites during cold upsetting.…”
Section: Introductionmentioning
confidence: 99%
“…They also reported that, the workability of a material purely depends on the amount of ductile fracture presented in the material 24 . The workability behavior for various ferrous and non-ferrous alloys and composites (Al-3.5%Al 2 [25][26][27][28][29][30] . In the present study, Al matrix composites with 2.5 weight percentage of TiO 2 and 2 & 4 weight percentage of graphite was synthesized through powder metallurgy route.…”
Section: Introductionmentioning
confidence: 99%