Soft flexural waves and self-localization of wrinkling modes of single- and few-layer graphene under compression in a compliant matrix

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
2
0

Year Published

2023
2023
2023
2023

Publication Types

Select...
1

Relationship

0
1

Authors

Journals

citations
Cited by 1 publication
(2 citation statements)
references
References 66 publications
0
2
0
Order By: Relevance
“…The depths of the gully-like wrinkles are ∼0.7 and ∼0.2 μm for the one-dimensional wrinkles (with 50% pre-strain in the X direction) and two-dimensional wrinkles (with 50% pre-strain in both X and Y directions), respectively (Figure g–i). The lower depth value in the two-dimensional wrinkles can be attributed to the Poisson’s effect of the shrunken PDMS substrate. , …”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation
“…The depths of the gully-like wrinkles are ∼0.7 and ∼0.2 μm for the one-dimensional wrinkles (with 50% pre-strain in the X direction) and two-dimensional wrinkles (with 50% pre-strain in both X and Y directions), respectively (Figure g–i). The lower depth value in the two-dimensional wrinkles can be attributed to the Poisson’s effect of the shrunken PDMS substrate. , …”
Section: Resultsmentioning
confidence: 99%
“…The lower depth value in the two-dimensional wrinkles can be attributed to the Poisson's effect of the shrunken PDMS substrate. 38,39 The periodicity of wrinkles in the film is an important factor affecting its tensile performance. The wavelengths of the periodic wrinkles in MXene films can be well-controlled by changing the pre-strain (ε pre ) of the PDMS substrates, which is defined as ε pre = ΔL/L, where L and ΔL are the initial length and the stretched length of the PDMS substrate, respectively.…”