Strontium Titanate (SrTiO3) with variation of sintering temperatures were prepared by co-precipitation methods. Sintering temperature were varied at 700 o C, 800 o C, and 900 o C for 4 hours. SrTiO3 samples were prepared by Strontium Nitrate and Titanium Tetrabutoxide. SrTiO3 samples were characterized by X-Ray Diffraction (XRD), Scanning Electron Microscopy (SEM), Resistance Capacitance Inductance (RCL) meter, and Sawyer Tower. SEM images show that the sintering temperatures could affect the grain size of SrTiO3. In addition, crystal size of SrTiO3 (110)
PENDAHULUANStrontium Titanat (SrTiO3) merupakan salah satu bahan metal oxide yang memiliki struktur perovskite kubik. SrTiO3 memiliki sifat fisika seperti paraelektrisitas, superkonduktivitas, dan fotokatalis [2] . Selain itu, SrTiO3 memiliki sifat kimia dan kestabilan fisik yang baik, serta sifat optik yang unggul [3] . Berdasarkan sifat-sifat tersebut SrTiO3 dikembangkan secara berkelanjutan untuk digunakan dalam beberapa aplikasi. Beberapa jenis aplikasi yang menerapkan bahan SrTiO3 adalah kapasitor, devais microwave, dan fotokatalis [5] .Penelitan mengenai SrTiO3 telah banyak dilakukan dengan berbagai metode seperti solid state, sol gel, hidrotermal dan co-precipitation. Dari beberapa metode tersebut, metode coprecipitation memiliki keunggulan yaitu homogenitas dan kontrol stokiometri yang bagus [4] .