Silver-Modified Nanosized Ferroelectrics as a Novel Photocatalyst

Abstract: Monodispersed ferroelectric BaTiO3 nanoparticles are synthesized as a model system to investigate the effect of ferroelectricity on a photocatalytic process. The results demonstrate that ferroelectricity can directly affect the photocatalytic activity due to promotion of the separation of photo-excited carriers by spontaneous polarization in ferroelectric materials. Moreover, Ag nanoparticles are attached on these BaTiO3 to further improve the photocatalytic property.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

3
62
0

Year Published

2016
2016
2021
2021

Publication Types

Select...
5
1

Relationship

0
6

Authors

Journals

citations
Cited by 108 publications
(65 citation statements)
references
References 33 publications
3
62
0
Order By: Relevance
“…The Ag/BTO thin films with different Ag/(Ag+BTO) ratios (abbreviated as Ag x /BTO, x = 0, 5,10,15,20,25,30, where x is the mole percent (mol%) of Ag) were prepared by a sol-gel and spin-coating method starting with barium acetate (Ba(CH 3 COO) 2 /BTO films, the ultimate solution was spin-coated onto glass substrate with size of 2 cm × 2 cm at 500 rpm for 5 s and subsequently 3000 rpm for 15 s. Finally, the thin films were dried at 150 ℃ for 30 s and successively heated to 500 ℃ for 1 h. These sequences of coating and pyrolysis treatments were repeated for 10 times.…”
Section: Preparationmentioning
confidence: 99%
See 4 more Smart Citations
“…The Ag/BTO thin films with different Ag/(Ag+BTO) ratios (abbreviated as Ag x /BTO, x = 0, 5,10,15,20,25,30, where x is the mole percent (mol%) of Ag) were prepared by a sol-gel and spin-coating method starting with barium acetate (Ba(CH 3 COO) 2 /BTO films, the ultimate solution was spin-coated onto glass substrate with size of 2 cm × 2 cm at 500 rpm for 5 s and subsequently 3000 rpm for 15 s. Finally, the thin films were dried at 150 ℃ for 30 s and successively heated to 500 ℃ for 1 h. These sequences of coating and pyrolysis treatments were repeated for 10 times.…”
Section: Preparationmentioning
confidence: 99%
“…To determine the dispersion and size of the Ag NPs inside the films, TEM analysis was performed for the Ag 25 /BTO thin film as shown in Fig. 2.…”
Section: Phase Structure and Morphologymentioning
confidence: 99%
See 3 more Smart Citations