“…The surface was washed with fresh water, dried for 1 hour, then cleaned with acetone or alcohol, according to what is customary among scientific sources. After the cleaning process, a base layer primer was used to increase the adhesion, as a primer from (model thick primer filler, WURTH, Germany) [40,41]. The paint (heat resistance paint, model dr ferro, black color, turkey origin) was sprayed with the addition of thinner (Nitro Cellulose thinner, Jordan origin) having a mixing ratio of 1:1, after the process of mixing the nanomaterial, iron oxide with the thinner to be ready for paint.…”