DOI: 10.1016/0022-5088(83)90164-9
|View full text |Cite
|
Sign up to set email alerts
|

Role of misch metal in galvanizing with a Zn-5%Al alloy

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1

Citation Types

0
3
0

Year Published

1994
1994
2020
2020

Publication Types

Select...
5
2

Relationship

0
7

Authors

Journals

citations
Cited by 16 publications
(3 citation statements)
references
References 0 publications
0
3
0
Order By: Relevance
“…50 These additions are made to improve the wettability and fluidity of the molten bath without affecting the corrosion resistance of the coating. 51 The microstructure of Galfan is characterized by a two-phase structure, a zinc-rich eta ͑͒ proeutectoid phase surrounded by a eutectic type phase consisting of beta ͑␤͒ aluminum and eta ͑͒ zinc lamellae. 52 The amount of the proeutectic was calculated to be 18%.…”
Section: Resultsmentioning
confidence: 99%
“…50 These additions are made to improve the wettability and fluidity of the molten bath without affecting the corrosion resistance of the coating. 51 The microstructure of Galfan is characterized by a two-phase structure, a zinc-rich eta ͑͒ proeutectoid phase surrounded by a eutectic type phase consisting of beta ͑␤͒ aluminum and eta ͑͒ zinc lamellae. 52 The amount of the proeutectic was calculated to be 18%.…”
Section: Resultsmentioning
confidence: 99%
“…Atomic diameter difference between La/Ce and Zn is 0?65 and 0?53 A respectively, which leads to negative residual viscosity of the galvanising melts after RE addition. Viscosity of Zn (3?5 MPa s) is higher than that of La and Ce (2?65 and 3?20 MPa s respectively) at the melting points, therefore (x Zn m Zn zx Re m Re )vm Zn (2) According to equation ( 2), the viscosity of Zn melts will decrease after RE addition, i.e. the fluidity of the melts will be improved, leading to smaller coating thickness.…”
Section: Coating Thicknessmentioning
confidence: 99%
“…Investigation showed that small mischmetal additions (LazCe,0?5%) in hot dip Zn-5Al coating (Galfan) can improve the wetability and fluidity of bath and minimise the spangle structure without affecting the corrosion resistance of the coating. 2 In the present paper, the effect of RE on microstructure, Fe-Zn reaction and corrosion resistance of galvanised Zn-0?18Al coating are studied.…”
Section: Introductionmentioning
confidence: 99%