Abstract: The sap of urushi tree (Toxicodendron vernicifluum (Stokes) F.A. Barkley) has been used for coating materials and is known as urushi or oriental lacquer in East Asia. The potential of termite attacks against wood samples coated with four types of urushi: Ki-urushi, Sugurome-urushi, Kuro-Sugurome-urushi, and Bengara-urushi, in correlation with their chemical and mechanical properties was investigated in this study. Mortalities of the subterranean Formosan termite (Coptotermes formosanus Shiraki) after a 3-week … Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3

Citation Types

0
8
0

Year Published

2020
2020
2023
2023

Publication Types

Select...
7

Relationship

1
6

Authors

Journals

citations
Cited by 7 publications
(8 citation statements)
references
References 18 publications
0
8
0
Order By: Relevance
“…The main compositions of OL are catechol derivatives (50–65%), water (20–35%), polysaccharides (plant gums) (5–7%), nitrogenous compounds (2–5%), and approximately 1% of laccase [ 1 , 2 , 3 ]. For improving the curing speed, enhancing the film gloss and other properties of films and coatings, the OL is usually refined by stirring below 45 °C [ 3 , 4 ] or other modified processes [ 5 , 6 , 7 , 8 ]. When the water content of OL is reduced to about 3%, it is classified and named as refined oriental lacquer (ROL).…”
Section: Introductionmentioning
confidence: 99%
“…The main compositions of OL are catechol derivatives (50–65%), water (20–35%), polysaccharides (plant gums) (5–7%), nitrogenous compounds (2–5%), and approximately 1% of laccase [ 1 , 2 , 3 ]. For improving the curing speed, enhancing the film gloss and other properties of films and coatings, the OL is usually refined by stirring below 45 °C [ 3 , 4 ] or other modified processes [ 5 , 6 , 7 , 8 ]. When the water content of OL is reduced to about 3%, it is classified and named as refined oriental lacquer (ROL).…”
Section: Introductionmentioning
confidence: 99%
“…Oriental lacquer is a natural polymeric material with a water in oil (W/O) emulsion sap, which is obtained by tapping Rhus trees, specifically Rhus succedanea , found in Taiwan and Vietnam [ 1 , 2 ]. The sap of raw oriental lacquer must be refined by stirring under a temperature below 45 °C to reduce the water content to around 3% [ 3 , 4 ] or other refined processes [ 5 , 6 , 7 , 8 ] for shortening the curing time and improving the gloss and other film properties of the raw oriental lacquer. It is defined as a refined oriental lacquer (ROL).…”
Section: Introductionmentioning
confidence: 99%
“…Finally, the unsaturated double bonds, the side chains of urushiols, undergo autoxidative polymerization to form a highly cross-linked network film. Many different refined processes were used to promote the drying process of OL because improving the laccase-catalyzed polymerization takes a long drying time in the limited condition of humidity and temperature [3,[10][11][12]. These improved OL had distinct film properties and were widely applied on the arts and crafts, and generally named as refined oriental lacquer (RL).…”