“…PDMS membrane. The flat-sheet PDMS membranes were prepared by mixing the polymer and the crosslinking agent (TRV 615 A+B, Momentive, Columbus, Ohio) in 10:1 weight ratio [38]. The mixture was first degassed in a desiccator and then cast onto a polished aluminium plate at controlled thickness.…”