Recovery of nickel powder from copper bleed electrolyte of an Indian copper smelter by electrolysis

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

1
8
0
1

Year Published

2011
2011
2022
2022

Publication Types

Select...
6
2
1

Relationship

0
9

Authors

Journals

citations
Cited by 26 publications
(10 citation statements)
references
References 10 publications
1
8
0
1
Order By: Relevance
“…Over thirty kinds heavy metals can be recovered from aqueous solutions by EL, including many precious metals and heavy metals [5]. There are many researches about copper recovery by EL [6][7][8][9]. Meanwhile the ED for acidic aqueous solution that contains copper ions has been studied by several workers [10][11][12].…”
Section: Introductionmentioning
confidence: 99%
“…Over thirty kinds heavy metals can be recovered from aqueous solutions by EL, including many precious metals and heavy metals [5]. There are many researches about copper recovery by EL [6][7][8][9]. Meanwhile the ED for acidic aqueous solution that contains copper ions has been studied by several workers [10][11][12].…”
Section: Introductionmentioning
confidence: 99%
“…Also, it was reported that the maximum nickel recovery from some polluting effluents was obtained within a pH interval of 4.66-5.55 at temperatures higher than 50 °C. 26,36 In addition, Njau and Janssen 37 report that the current efficiency goes through a maximum at about a pH of 5 when using a solution containing NiSO 4 and (NH 4 ) 2 SO 4 . Based on the above statements, a pH of 5.5 was chosen for the following tests.…”
Section: Resultsmentioning
confidence: 99%
“…3,6,7,14,[36][37][38][39][40][41][42][43] On an industrial scale, Ni electrowinning is performed at 60 °C from purified solutions containing chlorides or sulfates. 18 Likewise, the specific case of electrochemical production of nickel powder is carried out in the temperature range from 45 to 70 °C, 19,24,26 being the powders obtained at these temperatures very fine and easy to grind. However, excessively high temperatures, above 70 °C, should be avoided because Ni(II) hydroxide precipitation is favored.…”
Section: Resultsmentioning
confidence: 99%
“…They came to the conclusion that with this method it is possible to achieve a particle size of less than 5 nm and by increasing the temperature from 20 °C to 80 °C, the particle size will be in the range of 10 nm to 15 nm. Archana and et al [20] conducted a research titled recovery of nickel powder from copper electrolyte by electrolysis. They were able to recover 87% of the nickel, which increased to 99% under certain conditions.…”
Section: Introductionmentioning
confidence: 99%