Properties of the PLZTN x/54/46 (0.4≤x≤1.4) ceramic system

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1

Citation Types

0
3
0

Year Published

2010
2010
2023
2023

Publication Types

Select...
5
1

Relationship

0
6

Authors

Journals

citations
Cited by 6 publications
(3 citation statements)
references
References 20 publications
0
3
0
Order By: Relevance
“…The two Figures, 3(a, b) and 4(a, b) give the experimental results, the measurements of the dielectric parameters including the dielectric constant (εr) and the dissipation factor (tanδ) of the PLNZNCT ceramic sintered at 1200 °C, at the frequency of 1kHz depending on the temperature. According to previous studies, the doping of the acceptor ions in the perovskite crystal lattice decreases the dielectric constant and increases the curie temperature (Tc) [14]. The strongest dielectric response is that associated with the doped sample of 1mol %Cr.…”
Section: Dielectric Characterizationmentioning
confidence: 87%
“…The two Figures, 3(a, b) and 4(a, b) give the experimental results, the measurements of the dielectric parameters including the dielectric constant (εr) and the dissipation factor (tanδ) of the PLNZNCT ceramic sintered at 1200 °C, at the frequency of 1kHz depending on the temperature. According to previous studies, the doping of the acceptor ions in the perovskite crystal lattice decreases the dielectric constant and increases the curie temperature (Tc) [14]. The strongest dielectric response is that associated with the doped sample of 1mol %Cr.…”
Section: Dielectric Characterizationmentioning
confidence: 87%
“…But other author explain apparition of PL to order-disorder presence in the structure (Chen et al, 1989;Suárez-Gómez et al, 2009;Shannigrahi, 2007) distortion of oxygen octahedral fundamentally. Undoped PZT ceramics are seldom used.…”
Section: Luminescence In Pztmentioning
confidence: 94%
“…[37][38][39][40][41] The presence of acetylacetone has a positive effect on the gelation process as it can stabilize hydrolysis-sensitive precursors by complexation according to Refs. [14,42] and [43]. The result is a [29] with maximum occupation number in square brackets; bottom: c/a ratios of the lattice parameters of the rutile phase of samples of the Ir x Ti 1À x O 2 doping series prepared via a modified Pechini sol-gel route after calcination at T = 400 °C with reference values of the literature for TiO 2 and IrO 2 (blue) and the ideal ratio according to Pauling (red).…”
Section: Synthesis Protocol Of Ir X Ti 1àmentioning
confidence: 99%