1973
DOI: 10.1007/bf00791749
|View full text |Cite
|
Sign up to set email alerts
|

Production of properties of porous rolled materials

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

1982
1982
2015
2015

Publication Types

Select...
2
2

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(1 citation statement)
references
References 0 publications
0
1
0
Order By: Relevance
“…The supported nickel catalysts were prepared using a 0.1 mm thick porous nickel ribbon (pNirb) obtained by rolling nickel powder into a ribbon followed by calcination at 1200 °C in H 2 flow. 24 The ribbon nickel support had a specific surface area of 0.15 m 2 g −1 and a total pore volume of ca. 0.1 cm 3 g −1 .…”
Section: Catalyst Preparationmentioning
confidence: 99%
“…The supported nickel catalysts were prepared using a 0.1 mm thick porous nickel ribbon (pNirb) obtained by rolling nickel powder into a ribbon followed by calcination at 1200 °C in H 2 flow. 24 The ribbon nickel support had a specific surface area of 0.15 m 2 g −1 and a total pore volume of ca. 0.1 cm 3 g −1 .…”