“…The high reactivity of the (La, Sr)-containing electrodes with the conventional YSZ electrolyte facilitated extensive investigations of the LSM-based cathodes formed on the SDC [148][149][150][151], GDC [152], SSZ [151,153], LSGM [149], BaZr 0.8 Y 0.2 O 3 − δ (BZY20) [154], La 9.5 Si 6 O 26.25 [155], and La 27.44 W 4.56 O 55.68 (LWO56) [156] electrolytes as an alternative. The LSCF-based cathodes were formed on the SSZ [157], SDC [158,159], Ce 0.9 Gd 0.1 O 2 − δ (GDC10) [160][161][162], GDC [126,[163][164][165][166][167] Y 0.1 Ce 0.9 O 1.95 [168], Nd 0.2 Ce 0.8 O 3 − δ [169], SSZ [170], LSGM [171,172], GDC with LSGM [173], SDC with LSGM [174], BZY20 [175], BaZr 0.9 Y 0.1 O 3 − δ [176], BaZr 0.8 Yb 0.2 O 3 − δ (BZYb) [177], BaCe 0.7 Zr 0.1 Y 0.1 Yb 0.1 O 3 − δ (BCZYYb) [178][179][180][181][182], BaCe 0.7 Zr 0.1 Y 0.2 O 3 − δ (BCZY) [183][184][185], and BaCe 0.7 Zr 0.15 Y 0.15 O 3 − δ (BCZY15) [186] electrolytes.…”