2016
DOI: 10.1007/s00339-016-0224-3
|View full text |Cite
|
Sign up to set email alerts
|

Preparation of the flexible ZrO2/C composite nanofibrous film via electrospinning

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1

Citation Types

0
3
0

Year Published

2017
2017
2024
2024

Publication Types

Select...
5
1

Relationship

0
6

Authors

Journals

citations
Cited by 7 publications
(3 citation statements)
references
References 35 publications
0
3
0
Order By: Relevance
“…The stiff SiOC sample did not bend during the bending test, so no data were recorded. SiOC‐1.0Pd exhibited the greatest softness with a low flexural modulus of 2.23 kPa, which is even lower than the reported ZrO 2 /C nanofibers . Typical stress‐strain curves of the membranes are presented in Figure B.…”
Section: Resultsmentioning
confidence: 88%
See 2 more Smart Citations
“…The stiff SiOC sample did not bend during the bending test, so no data were recorded. SiOC‐1.0Pd exhibited the greatest softness with a low flexural modulus of 2.23 kPa, which is even lower than the reported ZrO 2 /C nanofibers . Typical stress‐strain curves of the membranes are presented in Figure B.…”
Section: Resultsmentioning
confidence: 88%
“…The bending length ( l ) was recorded upon the edge of the fiber mat get in contact with the slope. Then, the flexural rigidity ( B ) and the flexural modulus ( Q ) were calculated through the following equations: B=G×(0.5l)3×105×9.8 Q=12Bt3×103×9.8…”
Section: Resultsmentioning
confidence: 99%