Preparation of packing type catalysts AAO@Al/Meso-SiO2-SO3H for the dehydration of xylose into furfural

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
5
0

Year Published

2018
2018
2023
2023

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 15 publications
(6 citation statements)
references
References 43 publications
1
5
0
Order By: Relevance
“…Figure S1A shows the small-angle XRD patterns of thus-synthesized functionalized and pure SBA-15 materials. All samples presented well-resolved reflections that could be indexed as the (100), (110), and (200) planes corresponding to the typical P6mm space group, which were in line with those of the bare SBA-15 support reported in a previous publication . It was implied that the two-dimensional (2D) hexagonal mesostructures of the pure SBA-15 material in the investigated samples were retained even after undergoing incorporation of only Zn atoms or both Zn atoms and organic −SO 3 H groups.…”
Section: Resultssupporting
confidence: 86%
“…Figure S1A shows the small-angle XRD patterns of thus-synthesized functionalized and pure SBA-15 materials. All samples presented well-resolved reflections that could be indexed as the (100), (110), and (200) planes corresponding to the typical P6mm space group, which were in line with those of the bare SBA-15 support reported in a previous publication . It was implied that the two-dimensional (2D) hexagonal mesostructures of the pure SBA-15 material in the investigated samples were retained even after undergoing incorporation of only Zn atoms or both Zn atoms and organic −SO 3 H groups.…”
Section: Resultssupporting
confidence: 86%
“…In DMSO-toluene-water (1:8:2, v:v:v) containing NaCl (4% w/v), 2 wt% corn straw, and 10 wt% SO 4 2− /Sn-TRP catalyst (mass ratio and substrate), the yield of furfural reached 77.8% at 190 • C in 3 h [37]. In toluene-water (1:2. v:v), AAO@Al/FDU-5-7.5E-SO 3 H catalyzed xylose to produce furfural in the yield of 66.2% at 160 • C in 4 h [38]. The solid lignin-based catalyst LC-1S was used to transform xylose into furfural in the yield of 65% at 175 • C within 3 h in methyl isobutyl ketone (MIBK) [39].…”
Section: Introductionmentioning
confidence: 99%
“…Hu et al obtained by these means of several mesoporous sulfonated catalysts of the FDU and SBA type. Their best catalyst (FDU-5-7.5E-SO 3 H) was able to convert almost all xylose (97%), rendering up to 81% yield to furfural at 160 • C. However, again, on successive reaction cycles, the yield to furfural decreased down to 60% after the fifth cycle [78].…”
Section: Dehydration Of Xylose To Furfuralmentioning