Preparation of nanosheets embedded ZnSe/Bi2Se3 core/shell quantum dots for the study of optical properties and antibacterial activity

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
4
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
7

Relationship

3
4

Authors

Journals

citations
Cited by 8 publications
(8 citation statements)
references
References 61 publications
0
4
0
Order By: Relevance
“…The absence of Bi peaks in the primary sample CBIS-0 and the presence of the same in the CBIS-4 sample confirm the Bi content variation. 44 Doping led to significant defect redistribution. Thus, it can be observed that with Bi addition, the peak intensity is reduced, possibly due to the creation of defects and disorder inside the system.…”
Section: Resultsmentioning
confidence: 99%
“…The absence of Bi peaks in the primary sample CBIS-0 and the presence of the same in the CBIS-4 sample confirm the Bi content variation. 44 Doping led to significant defect redistribution. Thus, it can be observed that with Bi addition, the peak intensity is reduced, possibly due to the creation of defects and disorder inside the system.…”
Section: Resultsmentioning
confidence: 99%
“…Another three models are specified by Ravindra, Herve–Vandamme, and Tripathy and are specified as follows n R = 4.084 [ 0.62 × E normalg ] n 2 = 1 + ( A E normalg + B ) 2 and n T = 1.73 × [ 1 + 1.9017 × normale 0.539 × E normalg ] …”
Section: Resultsmentioning
confidence: 99%
“…The PL spectra of the different samples of CuZnSe are shown in Figure 10(c) in the range of 500 to 900 nm wavelength. The intense peaks are present because of the emission from defect levels of the composition [68,69] . The intensity of the PL peaks depends on the variation of the Cu and Zn concentrations.…”
Section: Resultsmentioning
confidence: 99%
“…The intense peaks are present because of the emission from defect levels of the composition. [68,69] The intensity of the PL peaks depends on the variation of the Cu and Zn concentrations. From the figure, it was found that sample CuZnSe-2 has the lowest PL intensity, and sample CuZnSe-3 has the highest intensity.…”
Section: Absorbance Optical Bandgap Refractive Index Dielectric Const...mentioning
confidence: 99%