Preparation and luminescence of green-emitting ZnAl2O4:Mn2+ phosphor thin films

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
12
0

Year Published

2015
2015
2022
2022

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 33 publications
(14 citation statements)
references
References 35 publications
0
12
0
Order By: Relevance
“…According to the specific frequencies of the absorption peaks, the functional groups existing in the samples can be deduced. Peaks at 1633, 656, 552, and 493 cm −1 are present in all samples, and are assigned to the H-O-H bending vibration of adsorbed water19, Al-O symmetric stretching vibration (ν 1 )19202122, Al-O symmetric bending vibration (ν 2 )19202122, and Al-O asymmetric stretching vibration (ν 3 )2122, respectively. For sample S2, the peaks located at 1186 and 1117 cm −1 are attributed to the S=O asymmetric stretching vibration23 and the S-O symmetric stretching vibration2324, respectively.…”
Section: Resultsmentioning
confidence: 94%
“…According to the specific frequencies of the absorption peaks, the functional groups existing in the samples can be deduced. Peaks at 1633, 656, 552, and 493 cm −1 are present in all samples, and are assigned to the H-O-H bending vibration of adsorbed water19, Al-O symmetric stretching vibration (ν 1 )19202122, Al-O symmetric bending vibration (ν 2 )19202122, and Al-O asymmetric stretching vibration (ν 3 )2122, respectively. For sample S2, the peaks located at 1186 and 1117 cm −1 are attributed to the S=O asymmetric stretching vibration23 and the S-O symmetric stretching vibration2324, respectively.…”
Section: Resultsmentioning
confidence: 94%
“…[36] The absorption bands between 500 and 1000 cm À1 are related to the stretching and bending vibrations of the Al─O bonds. [37][38][39] The Al 3+ ions located at octahedral sites of AlO 6 and tetrahedral AlO 4 denote the bending modes in the range 750-850 cm À1 .…”
Section: Ultraviolet-visible Spectroscopy Analysismentioning
confidence: 99%
“…Different luminescent aluminates have been developed in the form of films. ZnAl 2 O 4 films have been doped with Eu, Tb, or Tm using an ultrasonic spray pyrolysis technique [43,44]; films doped with Mn have been produced using a sol-gel route [45]. Concerning strontium aluminates, a SrAl 2 O 4 polymorph has been obtained by sputtering, ion beam evaporation, ultrasonic spray pyrolysis, and pulsed laser deposition [46][47][48][49][50][51][52].…”
Section: Designing Strategies For Ceramic Luminescent Films By Modified Screen Printing Assisted By Molten Saltsmentioning
confidence: 99%