2015
DOI: 10.1016/j.jeurceramsoc.2015.03.012
|View full text |Cite
|
Sign up to set email alerts
|

Preparation and enhanced electrical properties of grain-oriented (Bi1/2Na1/2)TiO3-based lead-free incipient piezoceramics

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1

Citation Types

4
67
0
1

Year Published

2015
2015
2022
2022

Publication Types

Select...
8
1

Relationship

1
8

Authors

Journals

citations
Cited by 218 publications
(72 citation statements)
references
References 59 publications
4
67
0
1
Order By: Relevance
“…Interestingly, despite the results showing the electric-field-induced evolution of mixed phase compositions between BNT-5BT and BNT-11BT, optimal properties were still observed at around BNT-7BT as was reported by Takenaka et al 6 In addition, Ma et al 15 have reported electric-field-induced creation/modification of MPB in this material system by in situ TEM. The unusual phase transformation behaviour of BNT-100xBT compositions is of interest as it's been shown to provide a mechanism to so-called "giant" strain property or incipient piezoelectricity [16][17][18][19] in related BNTbased compositions.…”
mentioning
confidence: 99%
“…Interestingly, despite the results showing the electric-field-induced evolution of mixed phase compositions between BNT-5BT and BNT-11BT, optimal properties were still observed at around BNT-7BT as was reported by Takenaka et al 6 In addition, Ma et al 15 have reported electric-field-induced creation/modification of MPB in this material system by in situ TEM. The unusual phase transformation behaviour of BNT-100xBT compositions is of interest as it's been shown to provide a mechanism to so-called "giant" strain property or incipient piezoelectricity [16][17][18][19] in related BNTbased compositions.…”
mentioning
confidence: 99%
“…[45]. In piezoelectric applications (for example, in transducers or actuators), the large signal piezoelectric coefficient, d * 33 is one of critical parameters and can be calculated by the following formula [46]:…”
Section: Electromechanical Propertiesmentioning
confidence: 99%
“…It must be noted that the aspect ratio of typical layer-structured template crystals usually decreases significantly during topochemical reactions. [14][15][16] In addition, the degree of texturing is critically dependent on the sintering time, which commonly exceeds tens of hours. The long sintering time hinders the use of volatile elements.…”
Section: Introductionmentioning
confidence: 99%
“…The long sintering time hinders the use of volatile elements. 15,17 Given that the hysteresis in IPS originates from ferroelastic domain reorientation during an electric-field-induced relaxor-to-ferroelectric transition, one possible solution is the optimal utilization of electrostriction while suppressing the relaxor-to-ferroelectric transition. 4,[18][19][20] It is known that (Bi 1/2 Na 1/2 )TiO 3 -based incipient piezoceramics exhibit a comparatively high electrostrictive coefficient.…”
Section: Introductionmentioning
confidence: 99%