Preparation and characterization of a three dimensional porous poly(lactic-co-glycolic acid)/mesoporous silica nanoparticles scaffold by low-temperature deposition manufacturing

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1

Citation Types

0
3
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
4

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(3 citation statements)
references
References 43 publications
0
3
0
Order By: Relevance
“…Phase separation and freeze drying ◆ High porosity ◆ Difficult control of porous structure ◆ Limited pore size range PCL/Chitosan/Gel [201] Pore size (5-73 µm), porosity (≈79%) Compressive strength:≈2.5 MPa, compressive modulus:≈3.8 MPa PLGA/mesoporous silica nanoparticles (MSNs) [182] Big pore (431 µm), small pore (5.6 µm), porosity (85.9%) Compressive modulus:≈25.9 MPa Gelatin/biodegradable poly (glycerol-co-sebacic acid-co-L-lactic acid-co-polyethylene glycol) (PGSLP) [202] Porosity (68.93%) Compressive modulus: 120.67 kPa…”
Section: Not Mentionedmentioning
confidence: 99%
“…Phase separation and freeze drying ◆ High porosity ◆ Difficult control of porous structure ◆ Limited pore size range PCL/Chitosan/Gel [201] Pore size (5-73 µm), porosity (≈79%) Compressive strength:≈2.5 MPa, compressive modulus:≈3.8 MPa PLGA/mesoporous silica nanoparticles (MSNs) [182] Big pore (431 µm), small pore (5.6 µm), porosity (85.9%) Compressive modulus:≈25.9 MPa Gelatin/biodegradable poly (glycerol-co-sebacic acid-co-L-lactic acid-co-polyethylene glycol) (PGSLP) [202] Porosity (68.93%) Compressive modulus: 120.67 kPa…”
Section: Not Mentionedmentioning
confidence: 99%
“…The absorption band around at 869 cm −1 was attributed to -C-H bending vibrations [56]. The absorption peaks at 1080 and 1165 cm −1 were assigned to stretching vibration of -C-O and asymmetrical stretching of C-O-C ether group [42,[57][58][59]. The peak at 1045 cm −1 was corresponding to -OH bending in -CH(CH3)-OH end groups [60].…”
Section: Ftir Analysismentioning
confidence: 99%
“…An appropriate surface hydrophilicity promotes cell adhesion and proliferation on the scaffolds [57,58]. The water contact angle of experimental groups was calculated to assess whether the addition of CNT increased the hydrophilicity of the PLGA and PLGA/HA.…”
Section: Water Contact Angle Measurementmentioning