Polymer composites prepared by low-temperature post-irradiation polymerization of C2F4 in the presence of graphene-like material: synthesis and characterization

Abstract: Study of PTFE–microwave exfoliated graphene oxide (MEGO) composites synthesized using a low temperature post-irradiation polymerization technique. SEM images of MEGO (left) and PTFE–MEGO composite (right).

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

1
7
0

Year Published

2016
2016
2024
2024

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 23 publications
(8 citation statements)
references
References 49 publications
1
7
0
Order By: Relevance
“…To determine the DG in PMMA–g–PTFE, TGA was exerted. As shown in Figure 2 , the degradation temperature range of pristine PTFE is 490–610 °C while that for PMMA is 180–420 °C, in good agreement with previous reports [ 51 , 52 ]. It is clear that the degradation of PMMA and PTFE are independent from each other.…”
Section: Resultssupporting
confidence: 91%
“…To determine the DG in PMMA–g–PTFE, TGA was exerted. As shown in Figure 2 , the degradation temperature range of pristine PTFE is 490–610 °C while that for PMMA is 180–420 °C, in good agreement with previous reports [ 51 , 52 ]. It is clear that the degradation of PMMA and PTFE are independent from each other.…”
Section: Resultssupporting
confidence: 91%
“…The XRD pattern of the PAN nanofiber mat reveals a broad peak at the 2θ value of near 21° owing to the amorphous structure, which agrees well with the previous reports. , For the Cu microfiber mat, discernible diffraction peaks were observed at the 2θ values of 43.5°, 50.5°, and 61.4° that correspond to the (111), (200), and (220) planes of Cu, respectively. That indicates that the Cu electroplated on the surface of PAN nanofibers was not oxidized. , In the case of the PTFE (Teflon) mesh, one strong and three weak peaks appeared at the 2θ values of 17.7°, 31.8°, 37.1°, and 41.6°. , A broad peak associated with the amorphous PTFE structure was also exhibited at the 2θ value of 16.3°. , …”
Section: Resultsmentioning
confidence: 92%
“…31,32 In the case of the PTFE (Teflon) mesh, one strong and three weak peaks appeared at the 2θ values of 17.7°, 31.8°, 37.1°, and 41.6°. 33,34 A broad peak associated with the amorphous PTFE structure was also exhibited at the 2θ value of 16.3°. 33,35 Figure 3b shows the results of Raman spectral analysis of each specimen.…”
Section: Resultsmentioning
confidence: 92%
“…Polytetrafluoroethylene (PTFE) is a polymer with superior chemical inertness, excellent thermal stability, low friction property and good biocompatibility . On the basis of these outstanding properties, PTFE fibers have been processed into fabrics or felts for further applications such as filtration, biomedical products and seawater desalination .…”