Abstract: Starting with 3,3′,4,4′‐biphenyltetracarboxylic dianhydride and methyl aminobenzoate, we synthesized a novel rodlike imide‐containing monomer, N,N′‐bis[p‐(methoxy carbonyl) phenyl]‐biphenyl‐3,3′,4,4′‐tetracarboxydiimide (BMBI). The polycondensation of BMBI with dimethyl terephthalate and ethylene glycol yielded a series of copoly(ester imide)s based on the BMBI‐modified poly(ethylene terephthalate) (PET) backbone. Compared with PET, these BMBI‐modified polyesters had higher glass‐transition temperatures and hi… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

0
19
0

Year Published

2005
2005
2014
2014

Publication Types

Select...
6

Relationship

3
3

Authors

Journals

citations
Cited by 16 publications
(19 citation statements)
references
References 14 publications
0
19
0
Order By: Relevance
“…From Figure 2(b), it can be seen that the crystallization temperatures of branched PBS copolymers are all lower than that of neat PBS, and decrease gradually with the increasing of 1,2‐OD segments content, indicating that the introduction of 1,2‐OD segments hindered the crystallizability of PBS. The supercooling degree (Δ T = T m − T c ) is an important parameter for determining the crystallizability of polymers 27. Generally speaking, the larger Δ T value, the lower the crystallizability.…”
Section: Resultsmentioning
confidence: 99%
“…From Figure 2(b), it can be seen that the crystallization temperatures of branched PBS copolymers are all lower than that of neat PBS, and decrease gradually with the increasing of 1,2‐OD segments content, indicating that the introduction of 1,2‐OD segments hindered the crystallizability of PBS. The supercooling degree (Δ T = T m − T c ) is an important parameter for determining the crystallizability of polymers 27. Generally speaking, the larger Δ T value, the lower the crystallizability.…”
Section: Resultsmentioning
confidence: 99%
“…Polymers containing 3,3′‐diamino‐4,4′‐dihydroxydiphenylsulfone exhibited enhanced solubility compared with polymers containing 2,2‐bis(3‐amino‐4‐hydroxyphenyl) hexafluoropropane because of the insolubility of the former polymer in dimethyl sulfoxide (DMSO), N , N ‐dimethylformamide (DMF), N ‐methyl‐2‐pyrrolidone (NMP) and N , N ‐dimethylacetamide (DMAc) Rigid groups are incorporated to distort the regularity of the main chain , . The rigidities of these groups should not be significantly different from those of heterocyclic polymers.…”
Section: Introductionmentioning
confidence: 99%
“…Rigid groups are incorporated to distort the regularity of the main chain , . The rigidities of these groups should not be significantly different from those of heterocyclic polymers.…”
Section: Introductionmentioning
confidence: 99%
See 1 more Smart Citation
“…Polyimides are one of the most important commercial polymers because of their good thermal properties and mechanical properties 17,18. To our knowledge, the combination of polyesters and polyimides has achieved great success and yielded a series of new materials with high performance 19–23. Xiao et al19 modified poly(ethylene terephthalate) (PET) by the incorporation of imide structures.…”
Section: Introductionmentioning
confidence: 99%