“…During heating, in the temperature interval of 450-700 °C, thermal decomposition of kaolinite (dehydroxylation) occurs and can be described according to the equation (Heide and Földvari, 2006;Ondruška et al, 2015;Ptáček et al, 2010bPtáček et al, , 2011:…”