Plasma-enhanced atomic layer deposition of carbon films employing a cyclic process of N2/H2 plasma and α, α’-dichloro-p-xylene as a precursor

Liugang Hu,
Takayoshi Tsutsumi,
Nobuyoshi Kobayashi