Abstract:AA7075 is extensively used in aerospace, defense, automotive applications because of its high strength to weight ratio. Issues related to fusion welding and corrosion resistance are key problems associated with these alloys. Friction stir welding is an alternative welding technique that overcomes problems associated with fusion welding. In the present investigation, preliminary studies were done on pitting corrosion behavior of AA7075 friction stir welds by adding silver along the weld joint line. Silver paste… Show more
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.