Pit sump drainage thickening to remove saponite rock suspension

Abstract: Advanced water supply systems for industrial enterprises represent complex facilities that include the supply of fresh water and its preparation for the process, treatment, decontamination and disposal of waste water, disposal of the resulting residue, and often the organization of a closed water cycle. Designing and operating such facilities is a complex technical and environmental task, which must be solved using the best available technologies. The management system for the drainage waters generated in diam… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2021
2021
2021
2021

Publication Types

Select...
2

Relationship

0
2

Authors

Journals

citations
Cited by 2 publications
(1 citation statement)
references
References 0 publications
0
1
0
Order By: Relevance
“…Dynamic viscosity according to Brookfield is designed for testing highly viscous materials, including suspensions, emulsions, and polymers. Determination of dynamic viscosity was performed by means of a Brookfield DV2TLV viscometer using spindles for various viscosity ranges. The feed mixture for determining the viscosity was prepared as follows: polystyrene powder with a particle size of <100 μm was added to the decantoil in the required ratio and, with constant mixing by a magnetic mixer, was heated on a hotplate at a temperature of 200 °C for 120 min to form a homogeneous mixture.…”
Section: Methodsmentioning
confidence: 99%
“…Dynamic viscosity according to Brookfield is designed for testing highly viscous materials, including suspensions, emulsions, and polymers. Determination of dynamic viscosity was performed by means of a Brookfield DV2TLV viscometer using spindles for various viscosity ranges. The feed mixture for determining the viscosity was prepared as follows: polystyrene powder with a particle size of <100 μm was added to the decantoil in the required ratio and, with constant mixing by a magnetic mixer, was heated on a hotplate at a temperature of 200 °C for 120 min to form a homogeneous mixture.…”
Section: Methodsmentioning
confidence: 99%