Photocatalytic decolorization of Basic Blue 41 using TiO2-Fe3O4-bentonite coating applied to ceramic in continuous system

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1

Citation Types

0
3
0

Year Published

2020
2020
2023
2023

Publication Types

Select...
6

Relationship

1
5

Authors

Journals

citations
Cited by 9 publications
(3 citation statements)
references
References 18 publications
0
3
0
Order By: Relevance
“…A. Photocatalyst Characterization XRD characterization of photocatalysts has also been described in substantial details [31], [32]. The main peak on 2θ = 30.3° and 35,7 o refer to the crystal of the magnetite phase, and these were supported by 2θ = 30.…”
Section: Resultsmentioning
confidence: 99%
See 2 more Smart Citations
“…A. Photocatalyst Characterization XRD characterization of photocatalysts has also been described in substantial details [31], [32]. The main peak on 2θ = 30.3° and 35,7 o refer to the crystal of the magnetite phase, and these were supported by 2θ = 30.…”
Section: Resultsmentioning
confidence: 99%
“…TiO 2 -Fe 3 O 4 -bentonite has been prepared according to the method described in our previous work [31], [32]. PANalytical PW 3373/00 X'Pert X-ray was used to observe the crystalline phase of the photocatalyst material (CuKα, 1.54 Å, radiation at 30 mA and 40 kV applied).…”
Section: B Methodsmentioning
confidence: 99%
See 1 more Smart Citation