2015
DOI: 10.3807/josk.2015.19.6.705
|View full text |Cite
|
Sign up to set email alerts
|

Opto-Electrochemical Sensing Device Based on Long-Period Grating Coated with Boron-Doped Diamond Thin Film

Abstract: The fabrication process of thin boron-doped nanocrystalline diamond (B-NCD) microelectrodes on fused silica single mode optical fiber cladding has been investigated. The B-NCD films were deposited on the fibers using Microwave Plasma Assisted Chemical Vapor Deposition (MW PA CVD) at glass substrate temperature of 475 ºC. We have obtained homogenous, continuous and polycrystalline surface morphology with high sp 3 content in B-NCD films and mean grain size in the range of 100-250 nm. The films deposited on the … Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

1
6
0

Year Published

2018
2018
2024
2024

Publication Types

Select...
7

Relationship

4
3

Authors

Journals

citations
Cited by 14 publications
(7 citation statements)
references
References 29 publications
1
6
0
Order By: Relevance
“…Experimental data from [13] were shown for comparison. The results obtained by the use of the meta-GGA method with FHI pseudopotentials are in close agreement with experiments [13][14], [16][17][18]. We can compare them to hybrid Becke three-parameter Lee-Yang-Parr (B3LYP) exchange functional [19], which is much more costly computationally.…”
Section: Faculty Of Electronics Telecommunications and Informatics supporting
confidence: 78%
“…Experimental data from [13] were shown for comparison. The results obtained by the use of the meta-GGA method with FHI pseudopotentials are in close agreement with experiments [13][14], [16][17][18]. We can compare them to hybrid Becke three-parameter Lee-Yang-Parr (B3LYP) exchange functional [19], which is much more costly computationally.…”
Section: Faculty Of Electronics Telecommunications and Informatics supporting
confidence: 78%
“…The seeding process included spinning of thin film from home-made nanodiamond suspension. The detonation nanodiamond (DND) slurry preparation procedure has been reported in the literature [10,26]. The power of microwaves was kept at 1300 W. Substrate temperature was kept at 700°C by an induction heater and measured by a thermocouple attached to the backside of a molybdenum substrate stage.…”
Section: Methodsmentioning
confidence: 99%
“…Boron doped diamond (BDD) film is an excellent electrode material which has a wide electrochemical window, from −1.25 V to 2.3 V in watery electrolytes, compared to a standard hydrogen * E-mail: matficek@pg.edu.pl electrode (SHE) [8] and chemical stability in harsh environments including great biocompatibility [9]. These properties make BDD excellent for use in multitudinous applications including electrochemical sensing [10,11], biosensing [12,13], electrocatalysis or wastewater treatment.…”
Section: Introductionmentioning
confidence: 99%
“…Pressure in the chamber was kept at 50 Torr during the process. The growth time was 3 h, producing B‐NCD films of a thickness less than 300 nm …”
Section: Methodsmentioning
confidence: 99%