Nickel Colloid Nanoparticles: Synthesis, Characterization, and Magnetic Properties

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

1
6
0

Year Published

2020
2020
2024
2024

Publication Types

Select...
6
1

Relationship

0
7

Authors

Journals

citations
Cited by 14 publications
(7 citation statements)
references
References 49 publications
1
6
0
Order By: Relevance
“…In addition of Ni(OH) 2 , the presence of NiO and Ni-NP also identified from the appearance of the UV-vis absorbance peak around 290 and 315 nm, respectively. [8,41,42] It is interesting to noticed that the peak corresponding to NiO and Ni-NP are significantly intense for the samples deposited at counter electrodes.…”
Section: Resultsmentioning
confidence: 94%
“…In addition of Ni(OH) 2 , the presence of NiO and Ni-NP also identified from the appearance of the UV-vis absorbance peak around 290 and 315 nm, respectively. [8,41,42] It is interesting to noticed that the peak corresponding to NiO and Ni-NP are significantly intense for the samples deposited at counter electrodes.…”
Section: Resultsmentioning
confidence: 94%
“…In a rapid process assisted by microwave and polyol, nickel nanoparticles were synthesized and stabilized in an aqueous emulsion of copolymers. This approach involves reducing a metal salt (NiCl2•6H2O) in the presence of a low concentration of hydrazine hydrate with the assistance of a commercial copolymer (latex) acting as both the reducing and stabilizing agents [45]. Synthesis of nickel nanoparticles using nickel chloride in ethylene glycol and hydrazine as reducing agent [46] can be represented as:…”
Section: Synthesis Of Nanoparticles and Nanocomposites In Polyolmentioning
confidence: 99%
“…The process of centrifugation was repeated 2-3 times. Then, the sample was dried overnight at 60 °C and calcined at 600 °C for 6 h [26,27] by following the hydrothermal reaction as shown in Eq. ( 1) to (3).…”
Section: Synthesis Of Ni-cuc Nanocompositementioning
confidence: 99%
“…For sample purification, put the sample into Teflon lined autoclave and placed into an electric furnace at 400 °C for 4 h. The sample was centrifuged at 4000 rpm with distilled water for 50 min and repeated the centrifugation 3-4 times. The sample was dried overnight at 60 °C and calcined at 600 °C for 6 h. [26,27]. A schematic diagram of the fabrication method is shown in Fig.…”
Section: Synthesis Of Ni-cuc Nanocompositementioning
confidence: 99%