Nanoindentation characterization of deformation and failure of aluminum oxynitride

Abstract: Fujita, T.; McCauley, J. W.; Singh, J. P.; and Chen, M. W., "Nanoindentation characterization of deformation and failure of aluminum oxynitride" (2011 Abstract A systematic study of the mechanical deformation and failure of transparent ceramic aluminum oxynitride (AlON) has been conducted using a depth-sensitive nanoindentation technique combined with transmission electron microscopy (TEM) and Raman spectroscopy. Although discrete displacement bursts appear in the load-depth profiles at high applied forces, a … Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

2
23
0

Year Published

2012
2012
2023
2023

Publication Types

Select...
8

Relationship

1
7

Authors

Journals

citations
Cited by 48 publications
(25 citation statements)
references
References 38 publications
2
23
0
Order By: Relevance
“…Anisotropic second-order elastic constants for AlON have been computed using first principles (Gazonas et al, 2010), as have pressure dependencies of second-order elastic coefficients (Batyrev et al, 2011). Recent indentation experiments suggest that AlON may be highly elastically anisotropic (Guo et al, 2011), in qualitative agreement with anisotropic constants used in the present work but contradicting previous work wherein nearly isotropic elastic constants were used (Clayton, 2011a). 4.…”
Section: Summary and Discussionsupporting
confidence: 62%
See 2 more Smart Citations
“…Anisotropic second-order elastic constants for AlON have been computed using first principles (Gazonas et al, 2010), as have pressure dependencies of second-order elastic coefficients (Batyrev et al, 2011). Recent indentation experiments suggest that AlON may be highly elastically anisotropic (Guo et al, 2011), in qualitative agreement with anisotropic constants used in the present work but contradicting previous work wherein nearly isotropic elastic constants were used (Clayton, 2011a). 4.…”
Section: Summary and Discussionsupporting
confidence: 62%
“…Transgranular fracture has been observed in AlON deformed at high rates (Paliwal et al, 2008;McCauley et al, 2009) and in static indentation experiments (Guo et al, 2011). 8.…”
Section: Summary and Discussionmentioning
confidence: 95%
See 1 more Smart Citation
“…ABF-STEM of amorphous shear bands. To illustrate the structure of the indentation-induced amorphous B 4 C, the cross-sectional TEM specimen was sliced from a residual indent using a focused ion beam milling (FIB) technique 26,27 . The detailed process has been illustrated in Fig.…”
Section: Resultsmentioning
confidence: 99%
“…17 Figure 6(b) depicts the experimental Raman spectra of AlON. 20 The Raman spectrum of cubic AlON is composed of a number of phonon modes at 304, 397, 626, 747, and 915 cm À1 related with 3T2g, Eg, and A1g modes of spinel. The modes can be seen in simulations of Raman activities (Figure 6(a)).…”
Section: Vibration Spectramentioning
confidence: 99%