2016
DOI: 10.1061/(asce)mt.1943-5533.0001532
|View full text |Cite
|
Sign up to set email alerts
|

Nanoindentation and Atomic Force Microscopy Investigations of Asphalt Binder and Mastic

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
2

Citation Types

0
7
0

Year Published

2018
2018
2023
2023

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 29 publications
(7 citation statements)
references
References 24 publications
0
7
0
Order By: Relevance
“…Besides, creep compliance is another performance criterion of a viscoelastic material, and therefore a great creep compliance means a weak deformation resistance. The formula of creep compliance can be drawn as Equation (11). 11) where J(t) is the creep compliance, in 1/MPa.…”
Section: Viscoelasticity States Of Interfacial Zonementioning
confidence: 99%
See 2 more Smart Citations
“…Besides, creep compliance is another performance criterion of a viscoelastic material, and therefore a great creep compliance means a weak deformation resistance. The formula of creep compliance can be drawn as Equation (11). 11) where J(t) is the creep compliance, in 1/MPa.…”
Section: Viscoelasticity States Of Interfacial Zonementioning
confidence: 99%
“…The formula of creep compliance can be drawn as Equation (11). 11) where J(t) is the creep compliance, in 1/MPa. The dissipated energy ratio is similar to the relaxation time for indicating the stress dissipation, and all three curves in Figure 13a show that the dissipated energy ratio increases with the increases in distance.…”
Section: Viscoelasticity States Of Interfacial Zonementioning
confidence: 99%
See 1 more Smart Citation
“…Over the past few decades, a large number of experimental methods have been proposed. Several precision measuring instruments such as atomic force microscopy [3][4][5] (AFM), scanning force microscope [6,7] (SFM), and nanoindentation, have been involved. Among the above methods, nano-indentation experiments [3,8] have been increasingly used in recent years.…”
Section: Introductionmentioning
confidence: 99%
“…With the advent of new technologies, capturing of rich information of materials at micro-or nanoscale levels has become easy in the recent time, and it has successfully been utilized in other natural science and engineering disciplines. Asphalt researchers have also recently advanced knowledge related to binder performance at much needed microscopic level, which is more important than meso-or macroscale [6][7][8]. Based on findings of the existing literature, it is clear that the behavior of asphalt pavement materials depends highly on their microstructure.…”
Section: Introductionmentioning
confidence: 99%