Nanocomposite membrane films on the basis of ether of cellulose and tetraethoxysilan

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1

Citation Types

1
11
0

Year Published

2011
2011
2024
2024

Publication Types

Select...
4
1

Relationship

3
2

Authors

Journals

citations
Cited by 5 publications
(12 citation statements)
references
References 13 publications
1
11
0
Order By: Relevance
“…Organic-inorganic EC films were prepared via the sol gel method at 50°C according to the procedure described in [14]. The ratio between alkoxide and the EC chain unit was varied from 1 : 1 to 4 : 1 (mol/mol) because, at larger amounts of alkoxides, brittle films were obtained.…”
Section: Objects and Analytical Methodsmentioning
confidence: 99%
See 2 more Smart Citations
“…Organic-inorganic EC films were prepared via the sol gel method at 50°C according to the procedure described in [14]. The ratio between alkoxide and the EC chain unit was varied from 1 : 1 to 4 : 1 (mol/mol) because, at larger amounts of alkoxides, brittle films were obtained.…”
Section: Objects and Analytical Methodsmentioning
confidence: 99%
“…The ratio between alkoxide and the EC chain unit was varied from 1 : 1 to 4 : 1 (mol/mol) because, at larger amounts of alkoxides, brittle films were obtained. During the synthesis, hydrochloric acid (0.15 moles per mole of alkoxide [14,17]) was used as a catalyst. The hydrolyzing agent was deion ized water, which was added to the THF solution of EC and alkoxide in an amount of 6 moles per mole of TEOS or 3 moles per mole of TTB because, in an acidic medium, the excess of water may facilitate rapid hydrolysis of TTB to form titanium dioxide [18].…”
Section: Objects and Analytical Methodsmentioning
confidence: 99%
See 1 more Smart Citation
“…For an example of films obtained by the sol-gel method with the use of different polymers and containing oxides, it has been shown [8,[12][13][14] that with an increase of the content of the latter, when the organo inorganic network becomes more dense, the degree of film swelling declines. The kinetic curves of the hybrid film swelling have the form typical of restrictedly swelling polymer systems, which network polymers are assigned to.…”
Section: The Behavior Of Hybrid Films In Aqueous Organic Mediamentioning
confidence: 99%
“…On the surface of hybrid films obtained with the use of different polymers [8,13,14], a nanosized rough ness was detected by the AFM method which is absent in films of the individual polymers. The dimension of the nanosized formations on the surface depended on the oxide nature and it was larger for films containing titania.…”
Section: Structure Of Hybrid Polymer-oxide Filmsmentioning
confidence: 99%