“…Furthermore, XRD pattern of the series of ZrW 2 O 8 NPs prepared under similar optimized conditions was given in Figure S2, which closely resemble with one another and no phase change was observed, which also indicated the reliability of the synthetic procedure. The average crystallite size of ZrW 2 O 8 NPs was obtained from Scherrer equation (Equation ) and it was found to be 42.7 nm 38 where, D , K , λ , β , and θ indicate mean crystallite size, K ‐shape factor (0.94), wavelength of the X‐ray beam, Full Width at Half Maximum (FWHM), and Bragg’s angle respectively.…”